05Invisible Technology

Why Do Batteries Gradually Lose Capacity?

Rechargeable batteries lose capacity because side reactions slowly use up lithium and damage the electrodes. Here is what happens inside, and what speeds it up.

Cylindrical lithium-ion battery cells seen from above

A new phone lasts all day; a few years later, the same phone needs a top-up by mid-afternoon. Laptops, cordless tools, e-bikes and electric cars all show the same pattern. Nothing has visibly broken, yet the battery holds less energy than it once did.

This gradual loss of capacity is one of the most studied problems in modern engineering, because it decides how long devices and vehicles stay useful and how much waste they create. The causes lie in chemical and mechanical changes deep inside the cell, and once you understand them, the advice about heat, full charges and fast charging starts to make sense.

The short answer

  • A lithium-ion battery stores energy by moving lithium ions between two electrodes. Capacity depends on how much lithium can make that journey and how much electrode material is available to hold it.
  • Unwanted side reactions, especially the slow growth of a film called the solid electrolyte interphase (SEI), trap lithium so it can no longer shuttle back and forth.
  • Repeated swelling and shrinking cracks electrode particles, and other reactions damage the positive electrode, so less material can store charge and internal resistance rises.
  • Heat, cold, long periods at a high state of charge and high charging currents all speed these processes up. Ageing continues slowly even when a battery is not being used.

The basic principle: a shuttle that slowly loses passengers

A lithium-ion cell has a negative electrode, usually made of graphite, a positive electrode made of a lithium metal oxide, and a liquid electrolyte between them. When you charge the battery, lithium ions travel from the positive electrode into the graphite. When you use it, they travel back, and electrons flow through your device to balance the charge.

In an ideal cell, every lithium ion would make that round trip forever. In practice, a small fraction is lost on every trip and with every hour that passes. Some lithium becomes locked into chemical by-products, some electrode material cracks or changes structure so it can no longer host lithium, and the cell’s internal resistance creeps up. Researchers group these changes into three broad effects: loss of lithium inventory, loss of active material and increased impedance (resistance).

How it works, step by step

  1. A protective film forms when the battery is new. On its first charge, the electrolyte reacts with the graphite surface to form the SEI, a thin solid layer that then shields the electrode from further attack. Forming it consumes some lithium; one review puts the first-cycle loss at roughly 10 per cent, which manufacturers allow for.
  2. The film keeps growing slowly. Electrolyte molecules can still seep through the layer, so it thickens over time, consuming more lithium.
  3. Electrodes breathe. Electrode particles expand and contract as lithium moves in and out. Over many cycles this flexing can crack them, exposing fresh surfaces where more SEI forms and disconnecting fragments that can no longer store charge.
  4. The positive electrode degrades. Particularly at high voltage and temperature, its crystal structure can change, oxygen can be released and metal ions can dissolve, migrate and speed up SEI growth on the other side.
  5. Under some conditions lithium plates out. Charging fast, in the cold or at very high states of charge can make lithium deposit as metal on the graphite surface instead of slipping inside it. Some of that lithium never returns to service.
  6. The losses add up. Less cyclable lithium, less active material and higher resistance together mean less usable capacity and more voltage drop under load.

The science behind it

The main mechanisms

A widely cited 2021 review of lithium-ion degradation identifies SEI growth, lithium plating, positive electrode decomposition and particle fracture as the principal mechanisms. The table summarises what each does and what tends to accelerate it.

Mechanism What it does Accelerated by
SEI growth Traps lithium in a growing surface film; raises resistance High temperature, high current
Lithium plating Deposits metallic lithium; some becomes permanently inactive; can form needle-like growths Low temperature, fast charging, high state of charge
Positive electrode decomposition Changes the electrode’s crystal structure; releases oxygen; dissolves metal ions High state of charge, high temperature
Particle fracture Cracks particles, disconnects material and exposes new surface for side reactions High current, extreme temperatures, large particles, silicon-rich electrodes

These processes interact. Cracking exposes new surface for SEI to grow on; SEI and metal deposits can clog the pores of the electrode, which makes plating more likely; and plated lithium in turn reacts to form more SEI. That coupling is one reason battery ageing can be hard to predict.

Why the slowdown is not linear

Because a thicker SEI layer makes it harder for electrolyte to reach the electrode, its growth slows over time and roughly follows the square root of time. A simplified way to write this is:

capacity loss from SEI ≈ k × √t

where t is time and k depends on temperature and other conditions. As an approximate illustration, if this mechanism alone cost a cell some capacity in its first year, it would take about four years to lose twice that amount, since √4 = 2. Real batteries are messier, because other mechanisms can take over later in life.

Temperature and state of charge

The same review describes temperature as the most significant stress factor, with departures from about 25 °C accelerating failure in both directions. Heat speeds up SEI growth and attacks the positive electrode; cold encourages lithium plating and cracking, especially while charging. A high state of charge, meaning a nearly full battery, speeds up unwanted side reactions and makes plating more likely. High currents add mechanical stress. Even nominally identical cells from the same production line can age at noticeably different rates.

Calendar ageing versus cycle ageing

Batteries age in two overlapping ways. Calendar ageing happens while the battery sits unused, driven mainly by temperature and state of charge. Cycle ageing comes from charging and discharging. Lifetime models used in research, such as those developed at the US National Renewable Energy Laboratory, account for both.

What manufacturers promise

Manufacturers usually describe battery life as the number of complete charge cycles before capacity falls to a set fraction of the original. Apple, for example, states these design targets under ideal conditions:

Device Design target Approximate average loss per complete cycle
iPhone 14 and earlier 80% of original capacity after 500 complete cycles about 0.04%
iPhone 15 and later 80% of original capacity after 1,000 complete cycles about 0.02%

The last column is a simple average (20 per cent spread over the stated cycles) for illustration only; real capacity loss does not fall by the same amount each cycle, and actual results depend on how a device is used and charged.

Real-world applications

Phones and laptops. Many devices now report a maximum capacity figure, and some manage charging to reduce the time spent at full charge. Apple, for example, gives 16–22 °C as the ideal ambient range for its devices and warns that using or charging them above 35 °C can permanently reduce battery lifespan; its phones also delay the final part of charging so they spend less time sitting at 100 per cent. If you are curious about how cable-free charging works, see our article on how wireless charging works.

Electric vehicles. To compete with conventional cars, vehicle batteries need to perform reliably for 10 to 15 years in many climates and driving patterns, according to the US National Renewable Energy Laboratory. Thermal management, the system that keeps the cells at suitable temperatures, is therefore a central part of how lifespan is designed for.

Grid storage. Large battery installations face the same chemistry, so operators weigh how hard to cycle the batteries against how quickly they will wear.

Common misconceptions

A battery only wears out when you use it

Calendar ageing continues while a battery sits on a shelf or in a drawer, and it is faster when the battery is warm and fully charged. Use is not the only clock running.

Battery life is just a matter of counting cycles

Cycle counts are a useful yardstick, but temperature, state of charge and charging current can change how much damage each cycle does. Two batteries with the same number of cycles can be in very different condition.

Fast charging is either harmless or always destructive

Higher currents do add stress and raise the risk of lithium plating, particularly in the cold. Device makers control charging to limit the stress; Apple, for instance, says its phones gradually reduce the charging current as the battery approaches full, partly to limit heat. The real effect depends heavily on conditions and on how well the charging is controlled.

Limitations and exceptions

This article focuses on lithium-ion batteries, which power most rechargeable consumer electronics and electric vehicles. Other chemistries, such as lead–acid or nickel–metal hydride, age through different mechanisms. Within lithium-ion, the details vary with electrode materials: nickel-rich positive electrodes and silicon-containing negative electrodes, for example, have their own weak points.

Battery ageing is also not only about capacity. Rising internal resistance can cause a device to shut down under heavy load even when some charge remains, and in rare cases damage such as lithium plating can lead to internal short circuits. If a battery becomes hot, swollen, damaged or behaves erratically, stop using and charging it and have it inspected or replaced by a qualified technician.

Frequently asked questions

Should I keep my phone charged to 100% all the time?

Spending long periods at a very high state of charge speeds up some ageing reactions, especially when the battery is warm. Many devices offer settings that limit or delay full charging for this reason.

Why does my battery drain faster in the cold?

Very cold conditions temporarily reduce how long a battery lasts, and performance returns to normal once it warms back into its normal operating range. Charging quickly in the cold is a separate concern, because it encourages lithium plating, which can cause permanent loss.

Can a degraded battery be restored?

Not in normal use. The lithium trapped in by-products and the cracked electrode material cannot be recovered by charging habits, so the practical remedy is replacement.

Does storing a battery at a cool temperature help?

Yes. Because heat accelerates the main ageing reactions, keeping a battery cool, and not fully charged, slows calendar ageing. Apple, for example, advises storing a device at around 50 per cent charge, switched off, in a cool, dry place below 32 °C.

References

  1. Apple. Maximising Battery Life and Lifespan.
  2. Apple Support. Charge and maintain your iPhone battery.
  3. Edge, J.S., O’Kane, S., Prosser, R. et al. Royal Society of Chemistry. Lithium ion battery degradation: what you need to know. 2021.
  4. Apple Support. About the battery and performance of iPhone 11 and later.
  5. National Renewable Energy Laboratory (archived page). Battery Lifespan.

Header photo: Vardan Papikyan on Unsplash.

David

Editor, The Hidden Layer

David edits The Hidden Layer. He writes and updates the site's explanations of everyday science and engineering, checks each article against its cited sources, and handles corrections.